XH56KMYUBVT (8-11)
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard |
Fe, % |
Si, % |
B, % |
Mg, % |
Mn, % |
Co, % |
Cr, % |
Ti, % |
Cu, % |
Ni, % |
V, % |
Al, % |
Ce, % |
P, % |
C, % |
S, % |
Nb, % |
Nd, % |
La, % |
Mo, % |
W, % |
| GOST 5632-14 |
< 1 |
< 0.3 |
< 0.01 |
< 0.1 |
< 0.4 |
12.5–16 |
10–12 |
2.4–3 |
< 0.07 |
51.815–63.36 |
0.4–0.8 |
2.8–3.3 |
< 0.015 |
< 0.015 |
0.04–0.08 |
< 0.01 |
2.5–3 |
< 0.005 |
< 0.08 |
4–5 |
2–3 |
Information on suppliers
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| B |
% |
Bor |
| Mg |
% |
Magnesium |
| Mn |
% |
Manganese |
| Co |
% |
Cobalt |
| Cr |
% |
Chrome |
| Ti |
% |
Titan |
| Cu |
% |
Copper |
| Ni |
% |
Nickel |
| V |
% |
Vanadium |
| Al |
% |
Aluminium |
| Ce |
% |
Cerium |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Nb |
% |
Niobium |
| Nd |
% |
Neodymium |
| La |
% |
Lanthanum |
| Mo |
% |
Molybdenum |
| W |
% |
Tungsten |