Chemical composition
| Standard | Fe, % | Si, % | B, % | Mn, % | Co, % | Cr, % | Ti, % | Cu, % | Ni, % | V, % | Al, % | Ce, % | P, % | C, % | S, % | Nb, % | Mo, % | W, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| GOST 23705 - 79 | < 3 | < 0.6 | < 0.01 | < 0.5 | < 0.5 | 15–17 | 1.2–1.6 | < 0.07 | 60.118–70.6 | < 0.2 | 1.2–1.6 | < 0.025 | < 0.015 | < 0.05 | < 0.012 | < 0.2 | 3.5–4.5 | 8.5–10 |
Note: By agreement of the parties C <0.06%
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 23705 - 79 | |
| GOST 5632-72 | |
| TU 108.01.059-86 | |
| TU 108.02.027-79 | |
| TU 14-1-2481-78 | |
| TU 14-1-322-72 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| B | % | Bor |
| Mn | % | Manganese |
| Co | % | Cobalt |
| Cr | % | Chrome |
| Ti | % | Titan |
| Cu | % | Copper |
| Ni | % | Nickel |
| V | % | Vanadium |
| Al | % | Aluminium |
| Ce | % | Cerium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Nb | % | Niobium |
| Mo | % | Molybdenum |
| W | % | Tungsten |