Kunial A
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Copper, copper alloys | Copper-Nickel Alloys |
Chemical composition
| Standard | Fe, % | Mn, % | Cu, % | Ni, % | Al, % | Pb, % | Примеси, % |
|---|---|---|---|---|---|---|---|
| GOST 492-2006 | < 1 | < 0.5 | 78.598–85.7 | 12–15 | 2.3–3 | < 0.002 | < 1.9 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 492-2006 | |
| GOST 492-1973 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Примеси | % | Impurities |
| Mn | % | Manganese |
| Cu | % | Copper |
| Ni | % | Nickel |
| Al | % | Aluminium |
| Pb | % | Lead |