Kunial B (MHA6−1,5)
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Copper, copper alloys | Copper-Nickel Alloys |
Chemical composition
| Standard | Fe, % | Mn, % | Cu, % | Ni, % | Al, % | Pb, % | Примеси, % |
|---|---|---|---|---|---|---|---|
| GOST 492-2006 | < 0.5 | < 0.2 | 89.898–93.3 | 5.5–6.5 | 1.2–1.8 | < 0.002 | < 1.1 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 492-2006 | |
| GOST 492-1973 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Примеси | % | Impurities |
| Mn | % | Manganese |
| Cu | % | Copper |
| Ni | % | Nickel |
| Al | % | Aluminium |
| Pb | % | Lead |