MF10
for the production of ferrous alloys
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Copper, copper alloys | Copper-phosphorous alloys |
Chemical composition
| Standard | Bi, % | Sb, % | P, % | Cu + P, % |
|---|---|---|---|---|
| GOST 4515-93 | < 0.002 | < 0.002 | 9.5–11 | < 99.8 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 4515-93 | |
| DSTU 2530-94 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Bi | % | Bismuth |
| Sb | % | Antimony |
| P | % | Phosphorus |
| Cu + P | % | Copper + Phosphorus |