MNZHKT5-1-0.2-0.2 (ERCuNi5Fe1)
Wire for manual, semi-automatic gas-shielded welding copper-nickel alloys, copper-nickel alloys and copper and bronze, brass and steel (carbon, alloyed and corrosion-resistant) and surfacing on steel
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Copper, copper alloys | Copper-Nickel Alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Ti, % | Cu, % | Zn, % | Pb, % | C, % | Ni + Co, % |
|---|---|---|---|---|---|---|---|---|---|
| GOST 492-2006 | 1–1.4 | 0.15–0.3 | 0.3–0.8 | 0.1–0.3 | 90–93.45 | < 0.5 | < 0.005 | < 0.03 | 5–6.5 |
Information on suppliers
Mechanical properties at 20 °C
| Rolling | Standard | Size, mm | Tension | Classifiers | $$\sigma _{U}$$, $$MPa$$ | Treatment |
|---|---|---|---|---|---|---|
| Wire is hard. | GOST 16130 - 90 | 440 |
Standards
| Standard | Description |
|---|---|
| GOST 492-2006 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Ti | % | Titan |
| Cu | % | Copper |
| Zn | % | Zinc |
| Pb | % | Lead |
| C | % | Carbon |
| Ni + Co | % | Nickel + Cobalt |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |