MNTS12-24
goryachepresovannye parts; Alloy well deformed in the cold state, good spring properties.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Copper, copper alloys | Copper-Nickel Alloys |
Chemical composition
| Standard | Fe, % | Cu, % | Zn, % | Pb, % | Ni + Co, % |
|---|---|---|---|---|---|
| GOST 492-2006 | < 0.3 | 62–66 | 20.4–27 | < 0.05 | 11–13 |
Information on suppliers
Analogues
| Germany | USA |
|---|---|
| 2.073 | C75700 |
Standards
| Standard | Description |
|---|---|
| GOST 492-2006 | |
| GOST 492-1973 | |
| DSTU GOST 492:2007 |