NMC
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Si, % | Mg, % | Mn, % | Co, % | Cu, % | Zn, % | Ni, % | C, % | S, % |
|---|---|---|---|---|---|---|---|---|---|---|
| GOST 2171-90 | < 0.1 | < 0.1 | < 0.05 | 0.5–1 | < 0.5 | < 0.1 | < 0.002 | 98.093–99.5 | < 0.05 | < 0.005 |
Note: Pb + Zn + Cd + As + Sb + P + Bi < 0.008
Note: Ni: Ni + Co
Information on suppliers
Analogues
| Germany |
|---|
| NiMn1 |
| 2.4106 (NiMn1) |
| 2.4109 |
| 2.411 (NiMn2) |
Standards
| Standard | Description |
|---|---|
| GOST 2171-90 | GOST 2171-90 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mg | % | Magnesium |
| Mn | % | Manganese |
| Co | % | Cobalt |
| Cu | % | Copper |
| Zn | % | Zinc |
| Ni | % | Nickel |
| C | % | Carbon |
| S | % | Sulfur |