NMts1
grid control mercury rectifiers.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Nickel, nickel alloys | Nickel alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mg, % | Mn, % | Cu, % | C, % | S, % | Ni + Co, % |
|---|---|---|---|---|---|---|---|---|
| GOST 492-2006 | < 0.1 | < 0.1 | < 0.05 | 0.5–1 | < 0.1 | < 0.05 | < 0.005 | < 98.5 |
Information on suppliers
Analogues
| Hungary |
|---|
| NiMn1 |
Standards
| Standard | Description |
|---|---|
| GOST 492-2006 | |
| GOST 492-1973 | |
| DSTU GOST 492:2007 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mg | % | Magnesium |
| Mn | % | Manganese |
| Cu | % | Copper |
| C | % | Carbon |
| S | % | Sulfur |
| Ni + Co | % | Nickel + Cobalt |