S-Ni22
For details of pumps, valves, compressors, bushings, housings of turbochargers, exhaust piping details.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Cast iron | Nickel cast iron |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Cu, % | Ni, % | P, % | C, % |
|---|---|---|---|---|---|---|---|---|
| GOST 7769-82 | 66.42–76.5 | 1–3 | 1.5–2.5 | < 0.5 | < 0.5 | 21–24 | < 0.08 | < 3 |
Information on suppliers
Physical characteristics
| Temperature, °C | $$E\cdot 10^{9}$$, $$MPa$$ |
|---|---|
| 20 | 0.98 |
Mechanical properties at 20 °C
| Rolling | Standard | Size, mm | Tension | Classifiers | $$\sigma _{U}$$, $$MPa$$ | $$\sigma_{P}$$, $$MPa$$ | $$\epsilon_L$$, % | Treatment |
|---|---|---|---|---|---|---|---|---|
| Casting | GOST 7769-82 | 370–440 | 170–250 | 30 |
Brinell hardness number
| Rolling | Standard | Classifiers | Value, HBW |
|---|---|---|---|
| GOST 7769-82 | 130–170 |
Standards
| Standard | Description |
|---|---|
| GOST 7769-82 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Cu | % | Copper |
| Ni | % | Nickel |
| P | % | Phosphorus |
| C | % | Carbon |
Description of physical characteristics
| Parameter | Units of measurement | Description |
|---|---|---|
| $$E\cdot 10^{9}$$ | $$MPa$$ | Elastic modulus |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |
| $$\sigma_{P}$$ | $$MPa$$ | Proportionality limit |
| $$\epsilon_L$$ | % | Elongation at break (longitudinal) |