GI25
for the manufacture of castings
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Cast iron |
Gray cast iron |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
P, % |
C, % |
S, % |
| GOST 1412-85 |
93.05–94.7 |
1.4–2.2 |
0.7–1 |
< 0.2 |
3.2–3.4 |
< 0.15 |
Information on suppliers
Physical characteristics
| Temperature, °C |
$$E\cdot 10^{9}$$, $$MPa$$ |
$$\alpha\cdot 10^{6}$$, $$K^{-1}$$ |
$$\varkappa$$, $$\frac{W}{m\cdot K}$$ |
$$\rho$$, $$\frac{kg}{m^3}$$ |
$$c\cdot 10^{-3}$$, $$\frac{J}{kg\cdot K}$$ |
| 20 |
100 |
|
50 |
7200 |
|
| 100 |
|
10 |
|
|
0.5 |
Mechanical properties at 20 °C
| Rolling |
Standard |
Size, mm |
Tension |
Classifiers |
$$\sigma _{U}$$, $$MPa$$ |
Treatment |
| Casting |
GOST 1412-85 |
|
|
|
250 |
|
Brinell hardness number
| Rolling |
Standard |
Classifiers |
Value, HBW |
|
GOST 1412-85 |
|
156–260 |
Casting and technological parameters
Analogues
| Germany |
USA |
| GG25 |
A48-40B |
|
C1.35B |
|
No.35 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
Description of physical characteristics
| Parameter |
Units of measurement |
Description |
| $$E\cdot 10^{9}$$ |
$$MPa$$ |
Elastic modulus |
| $$\alpha\cdot 10^{6}$$ |
$$K^{-1}$$ |
Coefficient of thermal (linear) expansion (range 20°C–T) |
| $$\varkappa$$ |
$$\frac{W}{m\cdot K}$$ |
Coefficient of thermal conductivity (the heat capacity of the material) |
| $$\rho$$ |
$$\frac{kg}{m^3}$$ |
The density of the material |
| $$c\cdot 10^{-3}$$ |
$$\frac{J}{kg\cdot K}$$ |
The specific heat of the material (range 20°C–T) |
Description of mechanical properties
| Parameter |
Units of measurement |
Description |
| $$\sigma _{U}$$ |
$$MPa$$ |
Ultimate tensile strength |
Description of the casting and technological parameters
| Parameter |
Units of measurement |
Description |
| linear shrinkage |
% |
The difference between model dimensions and the model casting |