AMg4K1.5M
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Si, % | Be, % | Sn, % | Mn, % | Ti, % | Cu, % | Zn, % | Al, % | Pb, % | Примеси, % |
|---|---|---|---|---|---|---|---|---|---|---|---|
| GOST 1583-93 | < 0.3 | 1.3–1.7 | 0.002–0.004 | < 0.02 | 0.6–0.9 | 0.1–0.25 | 0.7–1 | < 0.1 | 95.606–97.298 | < 0.02 | < 0.1 |
Note: Casting methods:
Note: Z - sand casting
Note: B - Lost wax casting
Note: K - chill casting
Note: D - injection molding
Note: Mark designation:
Note: h - clean
Note: bees - high purity
Note: och - high purity
Note: l - casting alloys
Note: c - selective
Information on suppliers
Analogues
| Germany | USA |
|---|---|
| GK-AlMg5Si | EN AC-51400 |
Standards
| Standard | Description |
|---|---|
| GOST 1583-93 | |
| GOST Р 55375-2012 | |
| DSTU 2839-94 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Примеси | % | Impurities |
| Si | % | Silicon |
| Be | % | Beryllium |
| Sn | % | Tin |
| Mn | % | Manganese |
| Ti | % | Titan |
| Cu | % | Copper |
| Zn | % | Zinc |
| Al | % | Aluminium |
| Pb | % | Lead |