MNA6-1.5 (Kunial B)
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard |
Fe, % |
Mn, % |
Cu, % |
Ni, % |
Al, % |
Pb, % |
Примеси, % |
| GOST 492-2006 |
< 0.5 |
< 0.2 |
89.898–93.3 |
5.5–6.5 |
1.2–1.8 |
< 0.002 |
< 1.1 |