Heat resisting structural steel 20X25H13ATL
It is used for the manufacture of parts for furnaces operating at temperatures up to 1100 ° C in air and hydrocarbon atmospheres.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Heat resistant steels and alloys | Heat resistant high alloy steel |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ti, % | Cu, % | Ni, % | C, % | N, % |
|---|---|---|---|---|---|---|---|---|---|
| GOST 5632-14 | 57.92–63.69 | < 0.7 | 1–1.5 | 23–25 | 0.1–0.2 | < 0.3 | 12–14 | 0.13–0.2 | 0.08–0.18 |
Information on suppliers
Analogues
| Russia |
|---|
| Сталь 20Х25НН13АТЛ-ВД |
Standards
| Standard | Description |
|---|---|
| GOST 5632-14 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ti | % | Titan |
| Cu | % | Copper |
| Ni | % | Nickel |
| C | % | Carbon |
| N | % | Nitrogen |