Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Ni, % |
P, % |
C, % |
S, % |
Mo, % |
| TU 14-1-4968-91 |
39.985–49 |
< 0.4 |
1–2 |
23.5–26.5 |
23.5–26.5 |
< 0.02 |
< 0.08 |
< 0.015 |
3–4.5 |
Information on suppliers
Properties
| Property |
| According to TU 14-1-4968-91 Note Not regulated |
| Density: 8.02 g / cm3 |