TU 14-1-4968-91
Information about the standard
| Standard | TU 14-1-4968-91 |
|---|---|
| Country | CIS, Russia, Ukraine |
| Type of standard | ГОСТ ТУ |
| Materials | Alloy of iron with nickel 36NMGT, EP606, EP622, EP673, EP803, Sv-08H25N25M3, Sv-08H25N40M7, Sv-08H25N50M10, Sv-36NGMT |