Sv-08H25N40M7 (EP673)
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Materials for welding and soldering |
Steel welding wire |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Ni, % |
P, % |
C, % |
S, % |
Mo, % |
| TU 14-1-4968-91 |
21.485–30.5 |
< 0.4 |
1–2 |
23.5–26.5 |
32.485–47.515 |
< 0.02 |
< 0.08 |
< 0.015 |
6.5–8 |
Information on suppliers
Свойства
| Свойство |
| По ТУ 14-1-4968-91 Примечание Не нормируются |
| Плотность: 8.26 г/см3 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Ni |
% |
Nickel |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Mo |
% |
Molybdenum |