B124
For the manufacture of engine parts; sealed alloy.
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Aluminum, aluminum alloys |
Foundry aluminum alloys |
Chemical composition
| Standard |
Fe, % |
Si, % |
B, % |
Mg, % |
Mn, % |
Ti, % |
Cu, % |
Al, % |
| GOST 1583-93 |
< 0.3 |
8–11 |
0.01–0.1 |
0.15–0.35 |
0.1–0.3 |
0.1–0.3 |
3–4 |
83.65–88.64 |
Information on suppliers
Mechanical properties at 20 °C
| Rolling |
Standard |
Size, mm |
Tension |
Classifiers |
$$\sigma _{U}$$, $$MPa$$ |
$$\epsilon_L$$, % |
Treatment |
| Casting |
|
|
|
in chill mold |
400 |
2 |
|
| Casting |
|
|
|
in sandy form |
340 |
0.5 |
|
Brinell hardness number
| Rolling |
Standard |
Classifiers |
Value, HBW |
| Alloy |
|
|
110–120 |
Casting and technological parameters
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| B |
% |
Bor |
| Mg |
% |
Magnesium |
| Mn |
% |
Manganese |
| Ti |
% |
Titan |
| Cu |
% |
Copper |
| Al |
% |
Aluminium |
Description of mechanical properties
| Parameter |
Units of measurement |
Description |
| $$\sigma _{U}$$ |
$$MPa$$ |
Ultimate tensile strength |
| $$\epsilon_L$$ |
% |
Elongation at break (longitudinal) |
Description of the casting and technological parameters
| Parameter |
Units of measurement |
Description |
| linear shrinkage |
% |