VAL10 (AM4.5Kd)
For heat-resistant high-strength products.
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Aluminum, aluminum alloys |
Foundry aluminum alloys |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mg, % |
Mn, % |
Ti, % |
Cu, % |
Zn, % |
Al, % |
Cd, % |
| GOST 1583-93 |
< 0.15 |
< 0.1 |
< 0.05 |
0.35–0.8 |
0.15–0.3 |
4.5–5.1 |
< 0.1 |
93.1–94.93 |
0.07–0.3 |
Information on suppliers
Physical characteristics
| Temperature, °C |
$$\alpha\cdot 10^{6}$$, $$K^{-1}$$ |
$$\rho$$, $$\frac{kg}{m^3}$$ |
| 20 |
|
2800 |
| 100 |
25.1 |
|
Mechanical properties at 20 °C
| Rolling |
Standard |
Size, mm |
Tension |
Classifiers |
$$\sigma _{U}$$, $$MPa$$ |
$$\sigma_{Y}$$, $$MPa$$ |
$$\sigma_{0.5}$$, $$MPa$$ |
$$KCU\cdot 10^{3}$$, $$\frac{J}{m^2}$$ |
Treatment |
| Casting |
|
|
|
in sandy form |
40–430 |
300–320 |
4–7 |
100–130 |
|
| Casting |
|
|
|
in chill mold |
500 |
400 |
4 |
200 |
|
Brinell hardness number
| Rolling |
Standard |
Classifiers |
Value, HBW |
| Casting |
|
|
70–120 |
Casting and technological parameters
Analogues
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mg |
% |
Magnesium |
| Mn |
% |
Manganese |
| Ti |
% |
Titan |
| Cu |
% |
Copper |
| Zn |
% |
Zinc |
| Al |
% |
Aluminium |
| Cd |
% |
Cadmium |
Description of physical characteristics
| Parameter |
Units of measurement |
Description |
| $$\alpha\cdot 10^{6}$$ |
$$K^{-1}$$ |
Coefficient of thermal (linear) expansion (range 20°C–T) |
| $$\rho$$ |
$$\frac{kg}{m^3}$$ |
The density of the material |
Description of mechanical properties
| Parameter |
Units of measurement |
Description |
| $$\sigma_{Y}$$ |
$$MPa$$ |
Yield strength |
| $$\sigma_{0.5}$$ |
$$MPa$$ |
Tensile stress required to produce a total elongation of 0.5% |
| $$\sigma _{U}$$ |
$$MPa$$ |
Ultimate tensile strength |
| $$KCU\cdot 10^{3}$$ |
$$\frac{J}{m^2}$$ |
Impact toughness |
Description of the casting and technological parameters
| Parameter |
Units of measurement |
Description |
| linear shrinkage |
% |
The difference between model dimensions and the model casting |