VAL11
For the manufacture of shaped castings; corrosion resistant alloy.
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Aluminum, aluminum alloys |
Foundry aluminum alloys |
Chemical composition
| Standard |
Be, % |
Mg, % |
Mn, % |
Cr, % |
Ti, % |
Zn, % |
Zr, % |
Al, % |
| GOST 1583-93 |
0.07–0.15 |
6–7 |
0.1–0.2 |
0.005–0.15 |
0.1–0.3 |
2–2.5 |
0.1–0.3 |
89.4–91.62 |
Information on suppliers
Mechanical properties at 20 °C
| Rolling |
Standard |
Size, mm |
Tension |
Classifiers |
$$\sigma _{U}$$, $$MPa$$ |
$$\sigma_{P}$$, $$MPa$$ |
$$\epsilon_L$$, % |
Treatment |
| Casting |
|
|
|
in sandy form |
320–360 |
250–280 |
4–7 |
|
Casting and technological parameters
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Be |
% |
Beryllium |
| Mg |
% |
Magnesium |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Ti |
% |
Titan |
| Zn |
% |
Zinc |
| Zr |
% |
Zirconium |
| Al |
% |
Aluminium |
Description of mechanical properties
| Parameter |
Units of measurement |
Description |
| $$\sigma _{U}$$ |
$$MPa$$ |
Ultimate tensile strength |
| $$\sigma_{P}$$ |
$$MPa$$ |
Proportionality limit |
| $$\epsilon_L$$ |
% |
Elongation at break (longitudinal) |
Description of the casting and technological parameters
| Parameter |
Units of measurement |
Description |
| linear shrinkage |
% |
The difference between model dimensions and the model casting |