VAL12
For high-strength corrosion-resistant products; maximum working temperature: 150 ° C — long, 200 ° C — short-term.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Aluminum, aluminum alloys | Foundry aluminum alloys |
Chemical composition
| Standard | Fe, % | Si, % | Be, % | Mg, % | Ti, % | Cu, % | Zn, % | Zr, % | Al, % |
|---|---|---|---|---|---|---|---|---|---|
| GOST 1583-93 | < 0.3 | < 0.2 | 0.05–0.25 | 2–2.8 | 0.1–0.3 | 1–1.5 | 6.5–7.5 | 0.05–0.25 | 86.9–90.3 |
Information on suppliers
Mechanical properties at 20 °C
Brinell hardness number
Analogues
| USA |
|---|
| 7278A |
Standards
| Standard | Description |
|---|---|
| GOST 1583-93 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Be | % | Beryllium |
| Mg | % | Magnesium |
| Ti | % | Titan |
| Cu | % | Copper |
| Zn | % | Zinc |
| Zr | % | Zirconium |
| Al | % | Aluminium |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |
| $$\sigma_{P}$$ | $$MPa$$ | Proportionality limit |
| $$\epsilon_L$$ | % | Elongation at break (longitudinal) |