N02211
Classification
| Country | Section | Category |
|---|---|---|
| USA | Nickel and Nickel Alloys | Nickel and Nickel Alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mg, % | Mn, % | Ti, % | Cu, % | Ni, % | C, % | S, % |
|---|---|---|---|---|---|---|---|---|---|
| UNS | < 0.2 | < 0.15 | 0.01–0.08 | 4.25–5.25 | 0.01–0.05 | < 0.15 | < 93.7 | < 0.2 | < 0.015 |
Information on suppliers
Analogues
| Germany |
|---|
| 2.4116 (NiMn5) |
Standards
| Standard | Description |
|---|---|
| UNS |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mg | % | Magnesium |
| Mn | % | Manganese |
| Ti | % | Titan |
| Cu | % | Copper |
| Ni | % | Nickel |
| C | % | Carbon |
| S | % | Sulfur |