N08042
Classification
| Country |
Section |
Category |
| USA |
Nickel and Nickel Alloys |
Nickel and Nickel Alloys |
Chemical composition
| Standard |
Si, % |
Mn, % |
Cr, % |
Ti, % |
Cu, % |
Ni, % |
P, % |
C, % |
S, % |
Mo, % |
| UNS |
< 0.5 |
< 1 |
20–23 |
0.6–1.2 |
1.5–3 |
40–44 |
< 0.03 |
< 0.03 |
< 0.003 |
5–6.7 |
Information on suppliers
Analogues
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Ti |
% |
Titan |
| Cu |
% |
Copper |
| Ni |
% |
Nickel |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Mo |
% |
Molybdenum |