09H17N7YU (0Х17Н7Ю)
Device for the wing, control surfaces, and brackets running in seawater; austenitic steel — martensitic class
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant ordinary steel |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ni, % | Al, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|---|---|---|
| GOST 5632-72 | 72.68–76.5 | < 0.8 | < 0.08 | 16–17.5 | 7–8 | 0.5–0.8 | < 0.03 | < 0.09 | < 0.02 |
Information on suppliers
Mechanical properties at 20 °C
| Rolling | Standard | Size, mm | Tension | Classifiers | $$\sigma _{U}$$, $$MPa$$ | $$\sigma_{P}$$, $$MPa$$ | $$\epsilon_L$$, % | $$KCU\cdot 10^{3}$$, $$\frac{J}{m^2}$$ | Treatment |
|---|---|---|---|---|---|---|---|---|---|
| The plates | GOST 7350-77 | 830 | 735 | 12 | 490 | Hardened and tempered |
Analogues
| USA | Germany |
|---|---|
| S17700 | 1.4568 (X7CrNiAl17-7) |
Standards
| Standard | Description |
|---|---|
| GOST 5632-72 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ni | % | Nickel |
| Al | % | Aluminium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |
| $$\sigma_{P}$$ | $$MPa$$ | Proportionality limit |
| $$\epsilon_L$$ | % | Elongation at break (longitudinal) |
| $$KCU\cdot 10^{3}$$ | $$\frac{J}{m^2}$$ | Impact toughness |