EI696A (10H11N20T2R)
Classification
Country |
Section |
Category |
CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant alloys |
Chemical composition
Standard |
Fe, % |
Si, % |
B, % |
Mn, % |
Cr, % |
Ti, % |
Ni, % |
V, % |
Al, % |
P, % |
C, % |
S, % |
Mo, % |
W, % |
GOST 5632-14 |
60.042–69.7 |
< 1 |
< 0.008 |
< 1 |
10–12.5 |
2.3–2.8 |
18–21 |
< 0.2 |
< 0.8 |
< 0.03 |
< 0.1 |
< 0.02 |
< 0.3 |
< 0.2 |
Information on suppliers
Properties
Property |
Performance data Application temperature: <700 ° C Scaling temperature: 850 ° C |
Calculated Properties Density: 7.85 g / cm3 |
Note Turbine Parts Austenitic Steel Heat Resistant Steel |
Standards
Description of chemical elements
Element |
Units of measurement |
Description |
Fe |
% |
Iron |
Si |
% |
Silicon |
B |
% |
Bor |
Mn |
% |
Manganese |
Cr |
% |
Chrome |
Ti |
% |
Titan |
Ni |
% |
Nickel |
V |
% |
Vanadium |
Al |
% |
Aluminium |
P |
% |
Phosphorus |
C |
% |
Carbon |
S |
% |
Sulfur |
Mo |
% |
Molybdenum |
W |
% |
Tungsten |