EI481 (37H12N8G8MFB)
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant alloys |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Ti, % |
Ni, % |
V, % |
P, % |
C, % |
S, % |
Nb, % |
Mo, % |
W, % |
| GOST 5632-14 |
62.885–70.71 |
0.3–0.8 |
7.5–9.5 |
11.5–13.5 |
< 0.2 |
7–9 |
1.3–1.6 |
< 0.035 |
0.34–0.4 |
< 0.03 |
0.25–0.45 |
1.1–1.4 |
< 0.2 |
Information on suppliers
Properties
| Property |
| Performance data Application temperature: <630 ° C Scaling temperature: 750 ° C |
| Calculated properties Density: 7.8 g / cm3 |
| Note Austenitic steel Heat resistant steel Turbine disks |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Ti |
% |
Titan |
| Ni |
% |
Nickel |
| V |
% |
Vanadium |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Nb |
% |
Niobium |
| Mo |
% |
Molybdenum |
| W |
% |
Tungsten |