Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Co, % | Cr, % | Ti, % | Cu, % | Ni, % | V, % | Al, % | P, % | C, % | S, % | Nb, % | Mo, % | W, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| GOST 5632-14 | < 3 | < 0.8 | < 0.4 | < 0.2 | 19–22 | 0.35–0.75 | < 0.07 | 67.898–77.6 | < 0.2 | 0.35–0.75 | < 0.02 | < 0.1 | < 0.012 | 0.9–1.3 | 1.8–2.3 | < 0.2 |
Information on suppliers
Properties
| Property |
|---|
| Performance data Application temperature: <1050 ° C Scaling temperature: 1100 ° C |
| Calculated Properties Density: 8.46 g / cm3 |
| Note Turbine Parts Heat Resistant Alloy Heat Resistant Alloy |
Standards
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Co | % | Cobalt |
| Cr | % | Chrome |
| Ti | % | Titan |
| Cu | % | Copper |
| Ni | % | Nickel |
| V | % | Vanadium |
| Al | % | Aluminium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Nb | % | Niobium |
| Mo | % | Molybdenum |
| W | % | Tungsten |