EI835 (12H25N16G7AR)
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard |
Fe, % |
Si, % |
B, % |
Mn, % |
Cr, % |
Ti, % |
Ni, % |
V, % |
P, % |
C, % |
S, % |
Mo, % |
N, % |
W, % |
| GOST 5632-14 |
46.465–56.7 |
< 1 |
< 0.01 |
5–7 |
23–26 |
< 0.2 |
15–18 |
< 0.2 |
< 0.035 |
< 0.12 |
< 0.02 |
< 0.3 |
0.3–0.45 |
< 0.2 |
Information on suppliers
Analogues
| Germany |
USA |
| BGH 2.4951 |
SPEC MIL-E-21562 (EN6N) |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| B |
% |
Bor |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Ti |
% |
Titan |
| Ni |
% |
Nickel |
| V |
% |
Vanadium |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Mo |
% |
Molybdenum |
| N |
% |
Nitrogen |
| W |
% |