HN57MTVYU (EP590)
Details of special equipment.
blades, housing and other parts of turbines
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Heat resistant steels and alloys | Heat resistant alloys |
Chemical composition
| Standard | Fe, % | Si, % | B, % | Mn, % | Cr, % | Ti, % | Ni, % | Al, % | Ce, % | P, % | C, % | S, % | Mo, % | W, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| GOST 5632-72 | 8–10 | < 0.5 | < 0.005 | < 0.5 | 17–19 | 2.2–2.8 | 53.09–61.8 | 1–1.5 | < 0.01 | < 0.015 | < 0.07 | < 0.01 | 8.5–10 | 1.5–2.5 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 5632-72 | |
| TU 14-1-2222-77 | |
| GOST 5632-14 | |
| TU 14-1-1214-75 | |
| TU 14-1-2894-80 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| B | % | Bor |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ti | % | Titan |
| Ni | % | Nickel |
| Al | % | Aluminium |
| Ce | % | Cerium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Mo | % | Molybdenum |
| W | % | Tungsten |