HN67MVTYU (EI202, HN67MVTYU-VD, EP202, EP202-VD)
Blades, body, wheels, leafy parts of turbines, welded products, operating at temperatures up to 800 ° C.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Heat resistant steels and alloys | Heat resistant alloys |
Chemical composition
| Standard | Fe, % | Si, % | B, % | Mn, % | Cr, % | Ti, % | Ni, % | Al, % | Ce, % | P, % | C, % | S, % | Mo, % | W, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| GOST 5632-72 | < 4 | < 0.6 | < 0.01 | < 0.5 | 17–20 | 2.2–2.8 | 60.475–71.8 | 1–1.5 | < 0.01 | < 0.015 | < 0.08 | < 0.01 | 4–5 | 4–5 |
Information on suppliers
Physical characteristics
| Temperature, °C | $$\alpha\cdot 10^{6}$$, $$K^{-1}$$ |
|---|---|
| 100 | 12 |
| 200 | 12.3 |
| 300 | 13.5 |
| 400 | 13.6 |
| 500 | 13.6 |
| 600 | 14.4 |
| 700 | 14.8 |
| 800 | 15.2 |
| 900 | 16.2 |
Mechanical properties at 20 °C
| Rolling | Standard | Size, mm | Tension | Classifiers | $$\sigma _{U}$$, $$MPa$$ | $$\sigma_{Y}$$, $$MPa$$ | $$\psi$$, % | $$KCU\cdot 10^{3}$$, $$\frac{J}{m^2}$$ | d5, % | Treatment |
|---|---|---|---|---|---|---|---|---|---|---|
| Sheet | GOST 24982-81 | 930 | 550 | 15–18 | Hardening and tempering | |||||
| Rod | GOST 23705 - 79 | 930 | 550 | 18 | 343 | 16 | Quenching and aging |
Brinell hardness number
| Rolling | Standard | Classifiers | Value, HBW |
|---|---|---|---|
| Rod | GOST 23705 - 79 | Hardening, aging | 241–341 |
Standards
| Standard | Description |
|---|---|
| GOST 5632-72 | |
| GOST 23705 - 79 | |
| GOST 24982-81 | |
| GOST 5632-14 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| B | % | Bor |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ti | % | Titan |
| Ni | % | Nickel |
| Al | % | Aluminium |
| Ce | % | Cerium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Mo | % | Molybdenum |
| W | % | Tungsten |
Description of physical characteristics
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\alpha\cdot 10^{6}$$ | $$K^{-1}$$ | Coefficient of thermal (linear) expansion (range 20°C–T) |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| d5 | % | Elongation at break |
| $$\sigma_{Y}$$ | $$MPa$$ | Yield strength |
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |
| $$\psi$$ | % | Reduction in cross section on fracture |
| $$KCU\cdot 10^{3}$$ | $$\frac{J}{m^2}$$ | Impact toughness |