N70MFV (EP814A)
The chemical equipment with operation in salt to — those at higher. t-re conc. P-pax sulfuric, phosphoric, acetic, hydrogen halide, ion exchange resins, polypropylene. In the process of organic synthesis and pharmaceuticals. 9200 kg / m3. OZL-23.
weldments operating at elevated temperatures in corrosive environments (sulfuric acid, acetic acid, chlorides, etc.)
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ti, % | Ni, % | V, % | P, % | C, % | S, % | Mo, % | W, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|
| GOST 5632-72 | < 0.8 | < 0.1 | < 0.05 | < 0.3 | < 0.15 | 69.403–73.5 | 1.4–1.7 | < 0.015 | < 0.02 | < 0.012 | 25–27 | 0.1–0.45 |
Information on suppliers
Mechanical properties at 20 °C
| Rolling | Standard | Size, mm | Tension | Classifiers | $$\sigma _{U}$$, $$MPa$$ | $$\sigma_{P}$$, $$MPa$$ | $$\epsilon_L$$, % | Treatment |
|---|---|---|---|---|---|---|---|---|
| Sheet | GOST 24982-81 | 780 | 365 | 40 | Hardening of 1050-1090 ° C |
Analogues
| USA | Germany |
|---|---|
| HastelloyB-2 | 2.4617 (NiMo28) |
Standards
| Standard | Description |
|---|---|
| GOST 5632-72 | |
| GOST 3239-81 | |
| TU 14-1-2260-77 | |
| TU 14-1-4684-89 | |
| TU 14-1-2230-77 | |
| TU 14-1-1227-83 | |
| GOST 24982-81 | |
| GOST 5632-14 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ti | % | Titan |
| Ni | % | Nickel |
| V | % | Vanadium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Mo | % | Molybdenum |
| W | % | Tungsten |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |
| $$\sigma_{P}$$ | $$MPa$$ | Proportionality limit |
| $$\epsilon_L$$ | % | Elongation at break (longitudinal) |