GOST 20072-74
Information about the standard
| Standard |
GOST 20072-74 |
| Country |
CIS, Russia, Ukraine |
| Type of standard |
ГОСТ |
| Materials |
12H1MF, 12H8VF, 12MH, 15H5, 15H5VF, 15X5M, 18H3MV, 20H1M1F1BR, 20H1M1F1TR, 20H3MVF, 25H1M1F, 25H1MF, EI415, EI579 |
| Download |
Download |